BMA putty polyester
Evens out surface unevenness on metal.

A two-component, solvent-based epoxy with good hardness and chemical resistance, used as an economical primer to provide chemical protection and mechanical strength against environmental conditions.
ISO 9001:2015 · ISO 45001:2018 · ISO 14001:2015
BMA Epoxy Primer is a two-component, solvent-based epoxy with good hardness and chemical resistance. It is used as an economical primer to provide chemical protection and mechanical strength against environmental conditions. It is suitable for application on well-prepared indoor and outdoor concrete wall and floor substrates, as well as on metallic structures exposed to water immersion and mechanical impacts.
Data for BMA Epoxy Primer cross-linked with 25% by volume of its hardener
| Parameter | Norm / standard | Result |
|---|---|---|
| Total Solids, by weight (%) | ASTM D1259 | 80 |
| Total Solids, by volume (%) | ISO 3233 | 64.04 |
| Viscosity at 25 °C (Poises) | ASTM D562 | 30 |
| Specific Gravity (g/cm³) | ASTM D1475 | 1.6 |
| Total Volatile Organic Compound (VOC) (g/L) | ASTM D3960 | 318.89 |
| Hardener ratio by volume (%) | — | 25 |
| Pot life (hours) | — | 2 |
| Induction time (minutes) | — | 10 |
| Gloss Level (%) | — | Matt |
| Appropriate solvent | — | BMA Thinner Epoxy |
| Solvent ratio by volume (%) | — | 25 |
| Parameter | Norm / standard | Result |
|---|---|---|
| Recommended WFT (µm) | — | 75–150 |
| Recommended DFT (µm) | — | 50–90 |
| Theoretical Spreading Rate (m²/L) | — | 7.11–12.8 |
Add 25% hardener by volume.
Before applying BMA Epoxy Primer, complete all necessary pretreatment. The surface should be clean, dry and free of all contaminants (oils, agents, dust, dirt, etc.) to avoid the risk of surface failure.
For new steel, clean any oil or grease residues from the surface using SAMA chemical 3 in 1 phosphating additive (1L:35L water). Sand the substrate to Sa 2½ until smooth, then remove all sanding dust and let it dry before applying any primer. For painted steel, remove loose and peeling paint by mechanical methods such as sanding or sandblasting the entire surface until smooth, so the new coating can adhere properly. When the old paint is compatible with the new one, only light sanding is required. Then remove persistent dirt, sanding residues and zinc salts with a detergent solution and water. For non-ferrous metal (galvanized steel, aluminum, stainless steel, etc.), remove corrosion residues and, to promote adhesion of the subsequently applied coatings, use a thin layer (8–10 µm) of BMA Wash Primer to etch the substrate. If the surface is unetched or etching is not possible, sweep or brush blast clean it with a non-metallic abrasive to lightly roughen the surface. Let the surface dry before coating application. To even out surface unevenness, apply BMA putty polyester. For corrosion prevention, prime the cleaned surface directly.
Prepare the concrete substrate well to avoid any coating defects. For a new surface, ensure the concrete is completely cured for at least 30 days. For both fresh and old concrete, decontamination is required to remove any dust, oil, grease, laitance, fatty acids or other contaminants. Acid etching with Acid Solution is recommended; decontamination can also be done by detergent scrubbing, low-pressure water cleaning or steam. Rinse well with water after acid etching. After cleaning, fill and repair any surface irregularities (cracks, holes and pores) with the cementitious mixture. To prepare the cementitious mixture, first make an SBR Solution by mixing BMA SBR with water (1:5 by volume), then add the SBR Solution to the cement and sand until you reach the desired cementitious mixture. BMA puttypoxy can be used to repair light scratches. Allow the concrete substrate to dry, then check its moisture and pH. Ensure the pH is between 6 and 9, since alkalinity can affect and destroy paint adhesion. Make sure the moisture content does not exceed 4% (by weight); otherwise, the concrete surface is not a good candidate for painting.
Thoroughly mix 25% by volume of the hardener 1BM-HPE0800 with BMA Epoxy Primer. Just before application, let the mixture rest for 10 minutes to allow a complete chemical reaction between the components. Apply within the pot life of 2 hours at ambient temperature.
If thinning is necessary, use a maximum of 15% for brush or roller application, and up to 20% for airless spraying, of BMA Thinner Epoxy to achieve the required viscosity.
Apply BMA Epoxy Primer in a well-ventilated area where the humidity does not exceed 75% and the temperature is between 5 °C and 35 °C. Do not subject the product to heavy mechanical stress before it is fully cured. Overcoating can be done after 6 hours, for example with BMA Enamopoxy Economic cross-linked with 25% of its hardener 1BM-HPE0800. Let the substrate dry for 3 days before light foot traffic, 5 days before heavy foot traffic and 7 days before vehicle traffic.
The products this coating is specified alongside in the data sheet.
Evens out surface unevenness on metal.
Repairs light scratches in concrete.
A thin layer (8–10 µm) etches non-ferrous metal (galvanized steel, aluminum, stainless steel, etc.) to promote adhesion.
View in catalogRecommended for acid etching of concrete during decontamination; rinse well with water afterward.
25% by volume; let the mixture rest 10 minutes before application. Pot life 2 hours at ambient temperature.
If needed: up to 15% for brush or roller, up to 20% for airless spraying.
Example overcoat, applied after 6 hours, cross-linked with 25% of its hardener 1BM-HPE0800.
Cleans oil or grease residues from new steel, diluted 1L:35L water.
Mixed with water (1:5 by volume) to make the SBR Solution for the cementitious repair mixture.
View in catalogStore in undamaged, unopened containers. The product must be kept away from direct sunlight and any sources of heat or flame.
Contains volatile organic compounds (VOCs); avoid release into the environment. Dispose of in accordance with local environmental regulations. Prevent contamination of soil and waterways.
Harmful by inhalation, skin contact, and if swallowed. May cause allergic skin reactions, respiratory irritation, or eye damage. Prolonged exposure may affect the central nervous system.
Use only in well-ventilated areas. Wear appropriate personal protective equipment (PPE) including gloves, goggles, and a respirator. Avoid direct contact with skin and eyes. Do not eat, drink, or smoke while using the product.
Inhalation: Move to fresh air; seek medical attention if symptoms persist. Skin Contact: Wash immediately with soap and water. Remove contaminated clothing. Eye Contact: Rinse cautiously with water for several minutes. Seek medical advice. Ingestion: Do not induce vomiting. Rinse mouth and seek immediate medical assistance.
The theoretical spreading rate is 7.11–12.8 m² per liter at the recommended dry film thickness of 50–90 µm.
Yes. Mix with 25% hardener by volume. Allow an induction time of 10 minutes. The pot life is 2 hours.
BMA Thinner Epoxy, at 25% by volume.
Apply it in a well-ventilated area, with humidity no higher than 75%, and at a temperature between 5 °C and 35 °C.