BMA Elastic Putty 1BM-EPS
Fills and repairs cracks, holes and pores in cleaned concrete before coating.

BMA Water-Based Pool Insulator is an acrylic resin pool insulator formulated to enhance waterproofing and fill tiny cracks, giving a uniform coating for surfaces constantly exposed to water and moisture.
ISO 9001:2015 · ISO 45001:2018 · ISO 14001:2015
BMA Water-Based Pool Insulator is a water-based acrylic resin pool insulator formulated to enhance waterproofing and fill tiny cracks, providing a uniform coating for surfaces constantly exposed to water and moisture. It offers long-lasting protection against ultraviolet radiation, dirt adherence, ozone, rain and snow. Once dry, it exhibits high elasticity and does not crack due to expansion, shrinkage or structural subsidence.
Data for BMA Water Based Pool Insulator 1BM-RCW101:
The specifications on the data sheet are stated for the White variant (1BM-RCW101) only.
| Parameter | Norm / standard | Result |
|---|---|---|
| Total Solids, by weight (%) | ASTM D2369 | 60 |
| Total Solids, by volume (%) | ISO 3233 | 50 |
| Total Pigments, by weight (%) | ASTM D 3723 | 30 |
| Viscosity at 25 °C (P) | ASTM D562 | 40 |
| Specific Gravity (g/cm³) | ASTM D1475 | 1.3 |
| Spreading Rate (m²/L) | — | 2.4 |
Carry out all necessary pretreatment before applying BMA Water-Based Pool Insulator. The surface should be clean, dry and free of all contaminants (oils, dust, dirt, etc.) to avoid the risk of surface failure.
Prepare the concrete substrate well to avoid any coating defects. For new surfaces, make sure the concrete has fully cured for at least 30 days. Fresh and old concrete both need decontamination to remove any dust, oil, grease, laitance, fatty acids or other contaminants. Acid etching with a hydrochloric acid solution is recommended; decontamination can also be done by detergent scrubbing, low-pressure water cleaning or steam. Rinse well with clean water after acid etching. After cleaning, fill and repair any surface irregularities (cracks, holes and pores) with BMA Elastic Putty 1BM-EPS and allow it to dry. Check the moisture and pH of the substrate. Make sure the pH is between 6 and 9, since alkalinity can affect and destroy paint adhesion, and that the moisture content does not exceed 4% (by weight). Otherwise, the concrete surface is not a good candidate for painting.
If thinning is required, apply the first layer of BMA Water-Based Pool Insulator with a brush or roller after diluting it with 80 to 100% water, the second layer after diluting it with 40 to 50% water, and the third layer with 0 to 20% water.
Apply BMA Water-Based Pool Insulator in a well-ventilated area where the humidity does not exceed 85% and the temperature is between 10 °C and 40 °C.
The products this coating is specified alongside in the data sheet.
Fills and repairs cracks, holes and pores in cleaned concrete before coating.
Store in undamaged, unopened containers. The product must be kept away from direct sunlight and any sources of heat or flame.
Contains volatile organic compounds (VOCs); avoid release into the environment. Dispose of in accordance with local environmental regulations. Prevent contamination of soil and waterways.
Harmful by inhalation, skin contact, and if swallowed. May cause allergic skin reactions, respiratory irritation, or eye damage. Prolonged exposure may affect the central nervous system.
Use only in well-ventilated areas. Wear appropriate personal protective equipment (PPE) including gloves, goggles, and a respirator. Avoid direct contact with skin and eyes. Do not eat, drink, or smoke while using the product.
Inhalation: Move to fresh air; seek medical attention if symptoms persist. Skin Contact: Wash immediately with soap and water. Remove contaminated clothing. Eye Contact: Rinse cautiously with water for several minutes. Seek medical advice. Ingestion: Do not induce vomiting. Rinse mouth and seek immediate medical assistance.
The theoretical spreading rate is 2.4 m² per liter.
Apply it in a well-ventilated area, with humidity no higher than 85%, and at a temperature between 10 °C and 40 °C.